Effect of Galardin as Matrix Metaloproteinase Inhibitor on the Dentin Bonding Durability of Old and Current Generations of Adhesive Systems
Effect of Galardin on the Dentin Bonding Durability
Abstract
Objectives: This study aimed to evaluate the effect of Galardin as a specific matrix metalloproteinase (MMP) inhibitor on dentin bonding durability of different generations of adhesive systems.
Materials and Methods: An in vitro study was performed on 32 extracted sound human molars. The occlusal enamel was removed prior to random assignment of the teeth into 8 groups by adhesive type and application/no application of Galardin. Each group was subdivided into 2 subgroups with/without aging. Adhesives were applied after the application of Galardin in the respective groups according to the manufacturer's instructions, and composite resin was incrementally built up to a height of 6mm. After performing the aging protocols for the respective subgroups, the teeth were sectioned into bar-shaped samples with a cross-sectional area of 1mm². The micro-tensile band strength (µTBS) test was then performed. Data were analyzed by three-way ANOVA, Bonferroni and Games-Howell post-hoc tests, and Chi-square test (alpha=0.05).
Results: The type of adhesive system, aging, and Galardin application had statistically significant effects on µTBS (P<0.001). Application of Galardin increased the µTBS (P<0.001) while aging decreased it (P<0.001). The interaction effect of aging and type of adhesive system on µTBS was also statistically significant (P<0.001). The other two-way and three-way interaction effects were not statistically significant (P>0.05).
Conclusion: Application of Galardin increased the µTBS values both immediately and after 6 months irrespective of the adhesive system type. Aging significantly decreased the µTBS. Type of adhesive also significantly affected the µTBS.
2. Chaussain-Miller C, Fioretti F, Goldberg M, Menashi S. The role of matrix metalloproteinases (MMPs) in human caries. J Dent Res. 2006 Jan;85(1):22-32.
3. Nishitani Y, Yoshiyama M, Wadgaonkar B, Breschi L, Mannello F, Mazzoni A, et al. Activation of gelatinolytic/collagenolytic activity in dentin by self‐etching adhesives. Eur J Oral Sci. 2006 Apr;114(2):160-6.
4. Mazzoni A, Angeloni V, Sartori N, Duarte Jr S, Maravic T, Tjäderhane L, et al. Substantivity of carbodiimide inhibition on dentinal enzyme activity over time. J Dent Res. 2017 Jul;96(8):902-8.
5. Breschi L, Cammelli F, Visintini E, Mazzoni A, Vita F, Carrilho M, et al. Influence of chlorhexidine concentration on the durability of etch-and-rinse dentin bonds: a 12-month in vitro study. J Adhes Dent. 2009 Jun;11(3):191-8.
6. Tezvergil-Mutluay A, Mutluay MM, Gu L-s, Zhang K, Agee KA, Carvalho RM, et al. The anti-MMP activity of benzalkonium chloride. J Dent. 2011 Jan;39(1):57-64.
7. Breschi L. Chlorhexidine application to stabilize the adhesive interface: why and how. J Adhes Dent. 2013 Aug;15(5):492.
8. Carrilho M, Geraldeli S, Tay F, De Goes M, Carvalho RM, Tjäderhane L, et al. In vivo preservation of the hybrid layer by chlorhexidine. J Dent Res. 2007 Jun;86(6):529-33.
9. Hebling J, Pashley DH, Tjäderhane L, Tay FR. Chlorhexidine arrests subclinical degradation of dentin hybrid layers in vivo. J Dent Res. 2005 Aug;84(8):741-6.
10. Breschi L, Martin P, Mazzoni A, Nato F, Carrilho M, Tjäderhane L, et al. Use of a specific MMP-inhibitor (galardin) for preservation of hybrid layer. Dent Mater. 2010 Jun;26(6):571-8.
11. Galardy RE, Grobelny D, Foellmer HG, Fernandez LA. Inhibition of angiogenesis by the matrix metalloprotease inhibitor N-[2R-2-(hydroxamidocarbonymethyl)-4-methylpentanoyl)]-L-tryptophan methylamide. Cancer Res. 1994 Sep;54(17):4715-8.
12. Augé F, Hornebeck W, Decarme M, Laronze J-Y. Improved gelatinase a selectivity by novel zinc binding groups containing galardin derivatives. Bioorganic Med Chem Lett. 2003 May;13(10):1783-6.
13. Almahdy A, Koller G, Sauro S, Bartsch J, Sherriff M, Watson T, et al. Effects of MMP inhibitors incorporated within dental adhesives. J Dent Res. 2012 Jun;91(6):605-11.
14. Jacob SW, Wood DC. Dimethyl sulfoxide (DMSO) toxicology, pharmacology, and clinical experience. Am J Surg. 1967 Sep;114(3):414-26.
15. Dillingham R, Oakley B. Surface energy and adhesion in composite–composite adhesive bonds. J Adhesion. 2006 May;82(4):407-26.
16. Ebrahimi-Chaharom M-E, Abed-Kahnamoui M, Bahari M, Hamishehkar H, Gharouni M. Effect of different concentrations of specific inhibitor of matrix metalloproteinases on the shear bond strength of self-adhesive resin cements to dentin. J Clin Exp Dent. 2017 Mar;9(3):e431-6.
17. Muñoz MA, Sezinando A, Luque-Martinez I, Szesz AL, Reis A, Loguercio AD, et al. Influence of a hydrophobic resin coating on the bonding efficacy of three universal adhesives. J Dent. 2014 May;42(5):595-602.
18. Rosa WL, Piva E, Silva AF. Bond strength of universal adhesives: A systematic review and meta-analysis. J Dent. 2015 Jul;43(7):765-76.
19. Wagner A, Wendler M, Petschelt A, Belli R, Lohbauer U. Bonding performance of universal adhesives in different etching modes. J Dent. 2014 Jul;42(7):800-7.
20. Armstrong SR, Vargas MA, Fang Q, Laffoon JE. Microtensile bond strength of a total-etch 3-step, total-etch 2-step, self-etch 2-step, and a self-etch 1-step dentin bonding system through 15-month water storage. J Adhes Dent. 2003 Spring;5(1):47-56.
21. Baracco B, Fuentes MV, Garrido MA, González-López S, Ceballos L. Effect of thermal aging on the tensile bond strength at reduced areas of seven current adhesives. Odontology. 2013 Jul;101(2):177-85.
22. Deng D, Yang H, Guo J, Chen X, Zhang W, Huang C. Effects of different artificial ageing methods on the degradation of adhesive-dentine interfaces. J Dent. 2014 Dec;42(12):1577-85.
23. Gale MS, Darvell BW. Thermal cycling procedures for laboratory testing of dental restorations. J Dent. 1999 Feb;27(2):89-99.
24. De Munck J, Van Landuyt K, Peumans M, Poitevin A, Lambrechts P, Braem M, et al. A critical review of the durability of adhesion to tooth tissue: methods and results. J Dent Res. 2005 Feb;84(2):118-32.
25. Morresi AL, D'Amario M, Capogreco M, Gatto R, Marzo G, D'Arcangelo C, et al. Thermal cycling for restorative materials: does a standardized protocol exist in laboratory testing? A literature review. J Mech Behav Biomed Mater. 2014 Jan;29:295-308.
26. de Moraes IQS, do Nascimento TG, da Silva AT, de Lira LMSS, Parolia A, Porto ICCM. Inhibition of matrix metalloproteinases: a troubleshooting for dentin adhesion. Restor Dent Endod. 2020 May 22;45(3):e31.
27. Sai K, Shimamura Y, Takamizawa T, Tsujimoto A, Imai A, Endo H, et al. Influence of degradation conditions on dentin bonding durability of three universal adhesives. J Dent. 2016 Nov;54:56-61.
| Issue | Vol 23 (Continuously Published Article-Based) | |
| Section | Original Article | |
| Keywords | ||
| Dental Bonding Matrix Metalloproteinase Inhibitors N-(2(R)-2-(hydroxamidocarbonylmethyl)-4-methylpentanoyl)-L-tryptophan methylamide | ||
| Rights and permissions | |
|
This work is licensed under a Creative Commons Attribution-NonCommercial 4.0 International License. |